Author | Topic |

Location: Kita-Ku, Sapporo, Japan
Registered: January 2003
|
Re: Head Annodising
|
Sat, 17 July 2004 04:26

|
 |
i agree it would look pretty spiffy if you were to get it dyed red or blue 
but if you are after heat loss, then it would be more efficient to get grooves in the outer surface of the head.
the rate limiting step for heat loss will be the surface-air interface. if you increase the surface area... you could get 2-3 times the surface area with the right shape/deep enough grooves... you will increase the rate of heat loss...
would also look interesting... anyone got a CNC machine handy?
|
|
|